Engineering plastics machined to a drawing: the stock grades, the tests behind their data sheets, the sizes a plastic part holds and the care it needs at the machine.
Machining plastic looks like machining metal and behaves very differently. The material softens with heat, grows with temperature and moisture, and springs back when the fixture lets it go. The articles here follow each of those effects through the stock makers’ data and the published tests.
Stock Grades
Engineering plastic stock as it cuts on a mill or a lathe: the acetals, the nylons cast and extruded, PEEK plain and carbon-filled, PEI and the polyethylenes. Each piece reads the stock maker’s data sheet for what it promises a machined part and what it leaves to the drawing.
Unfilled and carbon-filled PEEK share a polymer but differ in stiffness, conductivity, tooling, cutting data and tolerance, so the grade belongs on the drawing.
How Unfilled and Carbon-Filled PEEK Stock Differ for Machined PartsUnfilled PEEK machines like a hard, stiff thermoplastic: short chips, little burr, high feed rates and fine finishes. Carbon-filled PEEK machines like a composite: abrasive to tools, sensitive to fiber direction, and best cut with carbide or diamond at lower speeds.
Cast and extruded PA6 share a name but not their stress, crystallinity, chips or moisture behavior, and a machined nylon part keeps changing size after the cut.
Cast or Extruded PA6 for a Machined PartCast PA6 is usually the better machining stock when the part is large, flat, stiff or close-toleranced. Extruded PA6 is the tougher, more elastic choice for smaller parts where impact strength and elongation matter more than the last hundredth of a millimeter.
UHMW-PE wears longest and HDPE holds shape better, and both need sharp tools, chip control and a stated measurement temperature to hold size.
UHMW-PE and HDPE Differences for Machined PartsBoth are polyethylene, and the difference starts with chain length. Mitsubishi describes its TIVAR 1000 Virgin UHMW-PE as setting the standard for ultra high molecular weight polyethylene shapes, with a combination of wear and corrosion resistance, a low-friction surface and excellent impact strength.
PEI holds stiffness and shape at heat, and it asks for dry cutting, careful fluids and an annealing decision before the first part is cut.
PEI Ultem Properties for Machined PartsPolyetherimide, PEI for short, is an amorphous thermoplastic, and Ensinger, which extrudes it into rod and plate, notes that it is commonly referred to as ULTEM plastic after the resin's trade name. Ensinger describes the material as having high mechanical strength and rigidity, exceptional creep resistance over a wide temperature range and very good hydrolysis resistance, and as inherently flame retardant with low smoke emission, which makes it a preferred material for aircraft interiors.
Homopolymer is stiffer and harder, copolymer is sold porosity-free with less water uptake and less thermal growth, and the stock a part is cut from decides which it inherits.
Acetal Homopolymer and Copolymer Differences in Machined PartsAcetal, the polyoxymethylene or POM family, reaches a machine shop as two chemistries. Homopolymer chains repeat one unit; copolymer chains carry two.
The tests behind the numbers on a plastic stock data sheet: tensile strength, heat deflection temperature, water absorption, Shore and Rockwell hardness, and the UL 94 flammability rating. Each piece says what the specimen was, how the figure was measured and how far it carries to a machined part.
Shore D and Rockwell values on plastic stock sheets rank surface hardness under named methods, cannot be converted into each other, and bind a supplier only when agreed.
What Shore D and Rockwell Numbers Mean on a Plastic Stock Data SheetBoth numbers rank how strongly a plastic resists a hard indenter pressed into its surface at room temperature. Neither is a strength, a wear rating or a design value.
ASTM D570 reports how much water a plastic takes up under immersion, and for machined nylon that weight gain turns into growth the drawing has to allow for.
What ASTM D570 Measures and Why Nylon Parts CareThe method determines the relative rate at which plastics absorb water when immersed. ASTM gives the test two jobs.
A flame rating belongs to a material, a color and a thickness, so the call-out has to name all three and the machined wall has to stay inside them.
What UL 94 Covers and What It Leaves OutThe UL standards catalog lists UL 94 as Tests for Flammability of Plastic Materials for Parts in Devices and Appliances, in its seventh edition. Its scope states that the requirements cover tests for flammability of polymeric materials used for parts in devices and appliances, and that they serve as a preliminary indication of acceptability with respect to flammability for a particular application.
Heat deflection temperature ranks materials under one test load and says nothing about how long a loaded part keeps its shape at a given heat.
What ASTM D648 MeasuresThe scope of ASTM D648 is one sentence long. It covers the determination of the temperature at which an arbitrary deformation occurs when specimens are subjected to an arbitrary set of testing conditions.
A tensile figure on a data sheet belongs to one bar, one speed and one reading, so the sheet has to name all three before the number guides a design.
What ASTM D638 CoversThe scope of ASTM D638, Standard Test Method for Tensile Properties of Plastics, is the determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped specimens, tested under defined conditions of pretreatment, temperature, humidity and testing machine speed. On astm.org the 2022 edition is listed as active.
The limits a machined plastic part holds, and why it drifts from them: tolerances by part size and drilled hole, thermal expansion between the machine and the gauge, the flatness of thin plates, and the surface finish each material and tool leaves. Each limit comes with its material and its check.
Measured roughness on machined plastics follows feed first, then tool edge and material, and a finish call-out needs its parameter, surface, direction and part condition.
What Surface Finish Machined Plastics Reach and What Sets ItTwo open studies give a measured range for ordinary turning and milling of tough engineering plastics. Turning HDPE and PA6 with a carbide insert produced average roughness (Ra) from about 2.1 µm (83 µin) to about 11 µm (439 µin) across the tested conditions.
Thin plastic plates bow when stress, heat, clamping or moisture act on one face more than the other, so flatness is planned through stock, sequence, rest and measurement.
Why Thin Machined Plastic Plates Lose FlatnessA thin plate loses flatness when the stresses on its two faces stop balancing. Mitsubishi Chemical Advanced Materials (MCAM) explains the mechanism in its machining guide: extrusion, molding and machining leave residual stresses inside a thermoplastic, and when material is removed or the part meets elevated temperatures, those stresses redistribute and cause warping or dimensional change.
Every machined plastic dimension has a temperature, and the material decides how many degrees of drift a given tolerance can absorb.
Thermal Expansion of Machined Plastic Parts per 10 DegreesThe coefficient of linear thermal expansion, CTE, is the fractional length change per degree. Plastic sheets print it in 10⁻⁶ per kelvin or in inches per inch per degree Fahrenheit, and the two convert by a factor of 1.8: one in/in/°F is 1.8 per °C.
Published plastic tolerances widen with feature size and split by polymer group, so a drawing has to state size, grade, temperature and rest.
Published Machining Tolerances by Feature Size and Material GroupTable 1 reproduces the Mitsubishi table for nine of its sizes, with inches beside each figure. The five groups are the guide's own: HDPE; the group that holds PET-P, PC, PEEK, PTFE 500, PPS, PEI, PPSU and PSU; the group that holds PA, POM and PTFE 207; PEEK with fillers; and PAI with PBI.
A hole in plastic tends to close in behind the drill, so its size depends on the tool's condition, the stage that finishes it and the temperature it is measured at.
Why Holes in Plastic Come Out Undersize and What Else Moves ThemA hole in plastic differs from one in metal in four ways, and each has a published source.
Machining plastic step by step: sharp tools and the speeds and feeds that keep chips carrying the heat away, workholding that grips without bending, deep holes drilled without melting or cracking, and annealing between roughing and finishing so the released stress does not move the finished dimensions.
Acetal, nylon and PEEK share wide published cutting windows, and the right point inside each depends on making a chip that carries heat out of the part.
Speeds and Feeds for Acetal, Nylon and PEEK in One TableTable 1 sets the published cutting data for the three materials side by side, from MCAM's 2026 guide and from Tangram Technology, a UK plastics engineering consultancy that publishes indicative values. MCAM groups unfilled PEEK with PET-P and PAI, and filled PEEK with the other reinforced grades; Tangram does not list PEEK.
Holes deeper than two diameters trap heat in plastic, so drill grind, peck cycle, coolant choice and cool-down decide whether the part cracks or holds its size.
How to Drill a Deep Hole in Plastic Without Melting or CrackingTreat any hole deeper than two diameters as a cooling problem first and a cutting problem second. Both Mitsubishi Chemical Advanced Materials (MCAM) and Ensinger name the same threshold: heat builds very easily once the depth passes twice the diameter.
Plastic parts distort under clamps that metal parts shrug off, so the hold, the support and the symmetry of the cut set the final size.
How to Hold a Plastic Part on a CNC MachineHold it on as much surface as the geometry allows, with the lowest force that keeps it from moving, and with every thin wall backed by something solid. That sentence compresses three recommendations that recur across the stock-shape makers' guides: light clamping, support under the cut, and distribution of the force by vacuum or soft jaws instead of point contact.
Plastic cuts best with sharp tools, high feeds and an open chip path, because the chip is the only exit the cutting heat has.
Tool, Speed and Feed for CNC Plastic MachiningUse a sharp tool with generous clearance, a feed rate as high as the surface allows, and a path that lets the chip leave. That is the common opening of the stock-shape guides.
Annealing between roughing and finishing trades oven days for flat, stable parts, and it pays only when stress, shape or tolerance demand it.
When a Machined Plastic Part Needs AnnealingA machined plastic part needs an intermediate anneal when it has tight tolerances, an asymmetric shape, or a large share of its blank removed, and when it does not need one the stock maker has already done the work. Ensinger states the starting condition: its semi-finished products are always annealed after production, which is why a first cut can start without a stress-relief step.
A machined plastic run from the blank to the shipped batch: how many blanks a run needs, the days resting, annealing and drying add, how a batch is inspected and recorded, and the quantity at which a molded part takes over. Everything is counted in parts and days.
A machined plastic part moves to an injection mold once its design, volume, geometry and material all allow it, and the move brings a new drawing, standard and qualification.
Four Conditions That Make the Move to a Mold Worth ItThe move makes sense when four conditions hold together.
A machined batch carries a UL 94 V-0 rating only through its record of grade, color, thickness, listing and lot, plus proof the shop cut it dry and thick enough.
What a UL 94 V-0 Record Covers for a Machined Plastic BatchThe record covers the material, not the part. Ensinger, a stock-shape maker, states that combustibility testing to UL 94 is generally performed on the raw material.
A machined run is sized from weeks and consumption, converted to plates and batches, and then matched to cutters and fixtures by run length.
How to Size a Machined Plastic RunCount the parts the program will consume until the next process delivers, add a spare for parts lost in testing, convert the total to blanks by nesting, and group the blanks into batches that share a rest, an oven load and a measuring session. Then choose the cutter and the fixture by the length of the run.
In a machined plastic order the cutting takes minutes, while resting, drying and heat treatment take days, so the drawing sets the lead time.
Where the Calendar Goes in a Machined Plastic OrderMost of the elapsed time in a machined plastic order is spent on stock preparation, resting, heat treatment, drying and measurement at a controlled temperature, and the cutting is a small fraction. When a part needs none of those steps, it goes from blank to finished in the machine time plus setup and deburring.
Inspecting machined plastic means stating the temperature, the probe force and the sample size, because a plastic part changes with all three.
How to Inspect a Batch of Machined Plastic PartsInspect the batch at a stated temperature, with a low-force or non-contact method for soft or thin parts, on a sample whose size is chosen in advance, and record the conditions with the results. Those four elements separate a measurement that can be repeated from one that cannot.