Extrusion Centerline

The extrusion centerline is the central axis or mid-plane of an extruded rod or plate, where internal stress and, in acetal, porosity concentrate.

Every Extrusion Centerline article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

The extrusion centerline is the central axis or mid-plane of an extruded rod or plate, where internal stress and, in acetal, porosity concentrate. Ensinger states that extrusion leaves a stock shape with internal stress in the center. Where a part sits relative to that line decides how it moves when cut.

Bow Effect

Mitsubishi shows a plate machined on one side only, which bows top and bottom about the centerline of the extrusion. Cutting one side releases more stress on that side than the other. The PEI article repeats the illustration for the high-temperature grades. Quadrant asks for balanced machining on both sides of the stock centerline.
Read More

Layout Remedy

Mitsubishi’s advice for extrusions that bow starts with the thickest plate. The extrusion line is then moved away from the machined features. Slots or grooves go into the opposite face, and the cuts are balanced on both sides. Pockets are cut in intermediate steps. Mitsubishi also asks the machinist to consider rod as well as plate, because the two forms put the centerline in different places.

Porous Core

In acetal the centerline also carries a seam of interconnected pores. Ensinger sells its copolymer stock as porosity-free and makes no such claim for its homopolymer. The seam causes weakness and leakage under pressure.

Test-Bar Location

The ASTM D638 article notes that a test bar from a thick plate is machined from somewhere inside the section. The data sheets do not say whether that was near a face or through the centerline. A part’s weakest line may therefore differ from the bar’s. A drawing that cares about the centerline can name the stock size and where the part sits in it.

Flatness and Warp of Thin Machined Plastic Plates

Thin plastic plates bow when stress, heat, clamping or moisture act on one face more than the other, so flatness is planned through stock, sequence, rest and measurement.

Why Thin Machined Plastic Plates Lose FlatnessA thin plate loses flatness when the stresses on its two faces stop balancing. Mitsubishi Chemical Advanced Materials (MCAM) explains the mechanism in its machining guide: extrusion, molding and machining leave residual stresses inside a thermoplastic, and when material is removed or the part meets elevated temperatures, those stresses redistribute and cause warping or dimensional change.

Cast and Extruded Nylon PA6 Stock for Machined Parts

Cast and extruded PA6 share a name but not their stress, crystallinity, chips or moisture behavior, and a machined nylon part keeps changing size after the cut.

Cast or Extruded PA6 for a Machined PartCast PA6 is usually the better machining stock when the part is large, flat, stiff or close-toleranced. Extruded PA6 is the tougher, more elastic choice for smaller parts where impact strength and elongation matter more than the last hundredth of a millimeter.

Holding Plastic Parts for CNC Machining Without Bending Them

Plastic parts distort under clamps that metal parts shrug off, so the hold, the support and the symmetry of the cut set the final size.

How to Hold a Plastic Part on a CNC MachineHold it on as much surface as the geometry allows, with the lowest force that keeps it from moving, and with every thin wall backed by something solid. That sentence compresses three recommendations that recur across the stock-shape makers' guides: light clamping, support under the cut, and distribution of the force by vacuum or soft jaws instead of point contact.

Machining Tolerances by Part Size for Engineering Plastics

Published plastic tolerances widen with feature size and split by polymer group, so a drawing has to state size, grade, temperature and rest.

Published Machining Tolerances by Feature Size and Material GroupTable 1 reproduces the Mitsubishi table for nine of its sizes, with inches beside each figure. The five groups are the guide's own: HDPE; the group that holds PET-P, PC, PEEK, PTFE 500, PPS, PEI, PPSU and PSU; the group that holds PA, POM and PTFE 207; PEEK with fillers; and PAI with PBI.

PEI Ultem Stock for CNC Machined Parts

PEI holds stiffness and shape at heat, and it asks for dry cutting, careful fluids and an annealing decision before the first part is cut.

PEI Ultem Properties for Machined PartsPolyetherimide, PEI for short, is an amorphous thermoplastic, and Ensinger, which extrudes it into rod and plate, notes that it is commonly referred to as ULTEM plastic after the resin's trade name. Ensinger describes the material as having high mechanical strength and rigidity, exceptional creep resistance over a wide temperature range and very good hydrolysis resistance, and as inherently flame retardant with low smoke emission, which makes it a preferred material for aircraft interiors.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.

Request a Quote