Tensile Strength

Tensile strength is the stress a plastic specimen carries in tension.

Every Tensile Strength article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Tensile strength is the stress a plastic specimen carries in tension. Sheets print it at yield, where the bar stops springing back, or at break. ASTM D638 is the method behind it on most stock sheets. Of all the lines on a sheet, it is the one that moves most between sources. A strength without its label, speed and specimen is hard to use.

Yield and Break Values

For a ductile plastic the two can differ widely. TIVAR 1000 UHMW-PE yields at 21.0 MPa (3,050 psi) and breaks at 40.0 MPa (5,800 psi). Spartech’s HDPE prints 31.0 MPa (4,500 psi). A design read from the UHMW-PE break figure would be disappointed, since the bar yielded at roughly half.
Read More

Spread Between Sheets

Acetal stock sheets give 60.7 to 76.5 MPa (8,800 to 11,100 psi). A strength printed with no yield or break label may be either, as Mitsubishi’s note says. Without the label, a difference of 6 MPa (870 psi) could be the material or the reading. PEI shows the same problem. Mitsubishi’s TIVAR bar prints 40.0 MPa by ASTM D638 and 19 MPa by ISO 527.

Test Conditions

D638 notes that crosshead speed and specimen thickness move the result. Mitsubishi’s sheet prints its specimen types and speeds. Glass changes the number too. PEI with 30 percent glass breaks at 168.9 MPa (24,500 psi), 1.6 times the unfilled figure.

Design Use

A sheet’s strength ranks materials. The designer applies a margin for corners, temperature and time that the sheet cannot give. A call-out names yield or break, the specimen, the speed and whether the value is typical or a lot minimum.

Machining PEEK Unfilled and Carbon-Filled Stock

Unfilled and carbon-filled PEEK share a polymer but differ in stiffness, conductivity, tooling, cutting data and tolerance, so the grade belongs on the drawing.

How Unfilled and Carbon-Filled PEEK Stock Differ for Machined PartsUnfilled PEEK machines like a hard, stiff thermoplastic: short chips, little burr, high feed rates and fine finishes. Carbon-filled PEEK machines like a composite: abrasive to tools, sensitive to fiber direction, and best cut with carbide or diamond at lower speeds.

Cast and Extruded Nylon PA6 Stock for Machined Parts

Cast and extruded PA6 share a name but not their stress, crystallinity, chips or moisture behavior, and a machined nylon part keeps changing size after the cut.

Cast or Extruded PA6 for a Machined PartCast PA6 is usually the better machining stock when the part is large, flat, stiff or close-toleranced. Extruded PA6 is the tougher, more elastic choice for smaller parts where impact strength and elongation matter more than the last hundredth of a millimeter.

UL 94 Flammability Ratings for Machined Plastic Parts

A flame rating belongs to a material, a color and a thickness, so the call-out has to name all three and the machined wall has to stay inside them.

What UL 94 Covers and What It Leaves OutThe UL standards catalog lists UL 94 as Tests for Flammability of Plastic Materials for Parts in Devices and Appliances, in its seventh edition. Its scope states that the requirements cover tests for flammability of polymeric materials used for parts in devices and appliances, and that they serve as a preliminary indication of acceptability with respect to flammability for a particular application.

ASTM D638 Tensile Strength on Plastic Stock Data Sheets

A tensile figure on a data sheet belongs to one bar, one speed and one reading, so the sheet has to name all three before the number guides a design.

What ASTM D638 CoversThe scope of ASTM D638, Standard Test Method for Tensile Properties of Plastics, is the determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped specimens, tested under defined conditions of pretreatment, temperature, humidity and testing machine speed. On astm.org the 2022 edition is listed as active.

PEI Ultem Stock for CNC Machined Parts

PEI holds stiffness and shape at heat, and it asks for dry cutting, careful fluids and an annealing decision before the first part is cut.

PEI Ultem Properties for Machined PartsPolyetherimide, PEI for short, is an amorphous thermoplastic, and Ensinger, which extrudes it into rod and plate, notes that it is commonly referred to as ULTEM plastic after the resin's trade name. Ensinger describes the material as having high mechanical strength and rigidity, exceptional creep resistance over a wide temperature range and very good hydrolysis resistance, and as inherently flame retardant with low smoke emission, which makes it a preferred material for aircraft interiors.

Acetal Homopolymer and Copolymer Stock for CNC Machined Parts

Homopolymer is stiffer and harder, copolymer is sold porosity-free with less water uptake and less thermal growth, and the stock a part is cut from decides which it inherits.

Acetal Homopolymer and Copolymer Differences in Machined PartsAcetal, the polyoxymethylene or POM family, reaches a machine shop as two chemistries. Homopolymer chains repeat one unit; copolymer chains carry two.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.

Request a Quote