Thickness

Thickness is the section dimension of plastic stock or a part that sets which test applies, which rating holds and how long oven steps take.

Every Thickness article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Thickness is the section dimension of plastic stock or a part that sets which test applies, which rating holds and how long oven steps take. It appears in every standard in these resources as a limit. It appears in the oven rules as a rate. A machined wall can leave the range its material was tested in.

Test Limit

ASTM D638 covers material up to 14 mm (0.55 in) thick, and thicker stock is machined down to make the specimen. Sheeting under 1.0 mm (0.04 in) belongs to ASTM D882. The standard notes that thickness changes the surface-to-volume ratio and may change the result. ASTM D648 applies to stock 3 mm (1/8 in) thick or more. Sheet from 1 to 3 mm (0.04 to 1/8 in) is tested as a composite.
Read More

Rating Thickness

UL 94 excludes parts thicker than 13.0 mm (0.51 in), apart from the radiant panel test. For HB, UL allows a burn rate of 40 mm/min (1.6 in/min) for 3 to 13 mm (0.12 to 0.51 in). Below 3 mm (0.12 in) it allows 75 mm/min (3.0 in/min). Spartech’s HDPE sheet rates HB only above 3.2 mm (0.125 in). UL’s Yellow Card lists each flame class against a minimum thickness, so one grade can earn one class thicker and another thinner.

Machined Wall Effect

A web milled to 1.5 mm (0.06 in) from stock rated at 3 mm (0.12 in) leaves the record and needs its own evidence. A part thicker than 13 mm (0.51 in) sits outside the vertical and horizontal tests. The paper claim ends where the evaluated specimen ended.

Effect on Process Time

Thickness sets oven time too. The annealing hold runs 10 minutes per millimeter of wall, though wall matters far less than the ramps. Röhm anneals acrylic for the thickness in millimeters divided by 3 hours, with a minimum of 2. Quadrant dries nylon, PBI and PAI for at least 24 hours per 3 mm (0.12 in). The PAI post-cure cycle is printed for walls up to 12 mm (0.47 in).

A Flame-Retardant Machined Plastic Batch and Its UL 94 V-0 Record

A machined batch carries a UL 94 V-0 rating only through its record of grade, color, thickness, listing and lot, plus proof the shop cut it dry and thick enough.

What a UL 94 V-0 Record Covers for a Machined Plastic BatchThe record covers the material, not the part. Ensinger, a stock-shape maker, states that combustibility testing to UL 94 is generally performed on the raw material.

Flatness and Warp of Thin Machined Plastic Plates

Thin plastic plates bow when stress, heat, clamping or moisture act on one face more than the other, so flatness is planned through stock, sequence, rest and measurement.

Why Thin Machined Plastic Plates Lose FlatnessA thin plate loses flatness when the stresses on its two faces stop balancing. Mitsubishi Chemical Advanced Materials (MCAM) explains the mechanism in its machining guide: extrusion, molding and machining leave residual stresses inside a thermoplastic, and when material is removed or the part meets elevated temperatures, those stresses redistribute and cause warping or dimensional change.

Shore D and Rockwell Hardness on Plastic Stock Data Sheets

Shore D and Rockwell values on plastic stock sheets rank surface hardness under named methods, cannot be converted into each other, and bind a supplier only when agreed.

What Shore D and Rockwell Numbers Mean on a Plastic Stock Data SheetBoth numbers rank how strongly a plastic resists a hard indenter pressed into its surface at room temperature. Neither is a strength, a wear rating or a design value.

Machining PEEK Unfilled and Carbon-Filled Stock

Unfilled and carbon-filled PEEK share a polymer but differ in stiffness, conductivity, tooling, cutting data and tolerance, so the grade belongs on the drawing.

How Unfilled and Carbon-Filled PEEK Stock Differ for Machined PartsUnfilled PEEK machines like a hard, stiff thermoplastic: short chips, little burr, high feed rates and fine finishes. Carbon-filled PEEK machines like a composite: abrasive to tools, sensitive to fiber direction, and best cut with carbide or diamond at lower speeds.

How Long Resting, Annealing and Drying Add to Machined Plastic Parts

In a machined plastic order the cutting takes minutes, while resting, drying and heat treatment take days, so the drawing sets the lead time.

Where the Calendar Goes in a Machined Plastic OrderMost of the elapsed time in a machined plastic order is spent on stock preparation, resting, heat treatment, drying and measurement at a controlled temperature, and the cutting is a small fraction. When a part needs none of those steps, it goes from blank to finished in the machine time plus setup and deburring.

Annealing Machined Plastic Parts Between Roughing and Finishing

Annealing between roughing and finishing trades oven days for flat, stable parts, and it pays only when stress, shape or tolerance demand it.

When a Machined Plastic Part Needs AnnealingA machined plastic part needs an intermediate anneal when it has tight tolerances, an asymmetric shape, or a large share of its blank removed, and when it does not need one the stock maker has already done the work. Ensinger states the starting condition: its semi-finished products are always annealed after production, which is why a first cut can start without a stress-relief step.

UL 94 Flammability Ratings for Machined Plastic Parts

A flame rating belongs to a material, a color and a thickness, so the call-out has to name all three and the machined wall has to stay inside them.

What UL 94 Covers and What It Leaves OutThe UL standards catalog lists UL 94 as Tests for Flammability of Plastic Materials for Parts in Devices and Appliances, in its seventh edition. Its scope states that the requirements cover tests for flammability of polymeric materials used for parts in devices and appliances, and that they serve as a preliminary indication of acceptability with respect to flammability for a particular application.

ASTM D638 Tensile Strength on Plastic Stock Data Sheets

A tensile figure on a data sheet belongs to one bar, one speed and one reading, so the sheet has to name all three before the number guides a design.

What ASTM D638 CoversThe scope of ASTM D638, Standard Test Method for Tensile Properties of Plastics, is the determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped specimens, tested under defined conditions of pretreatment, temperature, humidity and testing machine speed. On astm.org the 2022 edition is listed as active.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.

Request a Quote