A sample UL Yellow Card for a polycarbonate grade lists the same material three times: V-1 at 0.75 mm (0.030 in), V-0 at 1.0 mm (0.039 in) and V-0 at 3.0 mm (0.118 in). UL Solutions prints it in its guide to reading the card, and it makes a point that every flame-retardant machined part depends on. A UL 94 rating belongs to a material at a thickness, in a color, as tested. Any machined batch inherits that rating only as far as its paperwork can trace the parts back to it.
This article follows one kind of batch, machined from flame-retardant stock, through the record that has to travel with it. It uses flame-retardant UHMW-PE as the working example, because two stock makers publish V-0 grades of it and one of them changes the machining rules as well as the fire behavior.
What a UL 94 V-0 Record Covers for a Machined Plastic Batch
The record covers the material, not the part. Ensinger, a stock-shape maker, states that combustibility testing to UL 94 is generally performed on the raw material. UL Solutions, in turn, issues a Yellow Card when a polymeric material receives its Recognized Component Mark, and the card lists the flame class against the color and the minimum thickness at which it was earned.
A machined part made from that material carries a traceable link to the rating when four facts are recorded and agree.
- The exact grade and color of the stock, as named on the card or the maker’s sheet.
- The minimum thickness at which the grade holds V-0, against the thinnest wall of the part.
- Whether the grade is listed by UL or only stated by its maker to meet the classification.
- The lot of stock the batch was cut from, with its certificate.
Even then, the record supports a product approval rather than replacing it. UL’s sample card carries the statement that UL 94 small-scale data are intended solely for determining the flammability of plastic materials used in components and parts of end-product devices and appliances, where the acceptability of the combination is determined by UL.
A V-0 record on a machined batch is a chain: grade, color, thickness, listing and lot. Without one link, the part may burn like the material, but cannot show it.
How UL Records a Material’s Flame Class
UL describes UL 94 as twelve flame classifications assigned to materials from small-scale flame tests. Six apply to materials for enclosures, structural parts and insulators (5VA, 5VB, V-0, V-1, V-2 and HB), three to low-density foams, and three to thin films (VTM-0, VTM-1 and VTM-2). The vertical V ratings come from UL’s 50 W, 20 mm (0.79 in) vertical method, with the flame applied at least twice to a vertical specimen, with burning and afterglow times and dripping recorded. UL states that a VTM rating cannot be considered equivalent to a V rating, because the methods differ.
Conditioning comes before the flame. UL lists two days at 23 °C (73 °F) and 50 % relative humidity before the vertical tests and the 5V test. The specimens are molded from the plastic material, which is one reason the rating describes the material rather than a machined part.
The result is published on the Yellow Card. UL explains that the card is issued automatically with the Recognized Component Mark and that recognized materials appear in its Product iQ database. UL’s guide to color codes and abbreviations defines the columns a buyer reads. Table 1 sets them out.
| Column on the card | Meaning given by UL | What it fixes for the batch |
|---|---|---|
| Color | Color code of the recognized material; the sample card reads ALL | The batch is cut from stock in a color the card covers |
| Min Thk (mm) | Minimum thickness in millimeters | The thinnest wall of the part is at or above it |
| Flame Class | UL 94 flammability classification | V-0 for this article’s subject |
| HWI, HAI | Hot wire ignition, high arc ignition | Short-term ignition properties, where the end product needs them |
| RTI Elec, Imp, Str | Relative temperature index for electrical, impact and strength properties | Long-term thermal rating, where the end product needs it |
UL also issues a White Card for testing to international standards. Its sample lists a flammability class to IEC 60695-11-10 at a stated thickness, which UL describes as harmonized with UL 94. Both cards print a thickness beside every class.
Flame-Retardant UHMW-PE Grades for Machined Parts
Ordinary UHMW-PE burns. Two stock makers publish grades modified to reach V-0, aimed at bulk handling equipment where liners and wear strips may be exposed to combustion. Table 2 sets the published data side by side.
| Property | TIVAR BurnGuard UHMW-PE (Mitsubishi Chemical Advanced Materials) | Polystone M Flametech AST black (Röchling) | Polystone M flame retardant, ASTM sheet (Röchling) |
|---|---|---|---|
| Flame rating as printed | UL 94 V-0, thickness not printed | UL 94 V-0 at 3 mm and 6 mm (0.12 and 0.24 in) | not printed; MSHA approved for underground mining |
| Electrical character | Static dissipative | Antistatic; volume and surface resistivity 10⁹ Ω·cm and 10⁹ Ω | Surface resistivity above 10¹² Ω, volume above 10¹⁵ Ω·cm |
| Stock form and color | Plate; black-silver | Black | Not printed |
| Density, g/cm³ (lb/in³) | Not printed | above 0.99 (0.0358) | Not printed |
| Yield stress, ISO 527, MPa (ksi) | Not printed | above 20 (2.9) | Not printed |
| Shore D, ISO 868 | Not printed | above 63 | Not printed |
| Melting range | Not printed | 130 to 135 °C (266 to 275 °F) | 266 to 275 °F (130 to 135 °C) |
| Linear thermal expansion | Not printed | 150 to 230 × 10⁻⁶/K (83 to 128 × 10⁻⁶/°F) | 2 × 10⁻⁴ in/in/°F (3.6 × 10⁻⁴/K), ASTM D696 |
| Service temperature | Not printed | −200 to 80 °C (−328 to 176 °F) long term; 130 °C (266 °F) short term | 180 °F (82 °C) maximum in air |
| Vicat softening, ISO 306 method B | Not printed | 79 °C (174 °F) | Not printed |
The table shows how uneven the published record can be.
MCAM’s page states the V-0 rating without a thickness. Röchling’s ISO sheet gives the thicknesses but no UL file reference. The ASTM sheet for Röchling’s other flame-retardant grade cites a mining approval and no UL class at all. None of the three, as published, is a Yellow Card.
Listed Material Against a Material That Complies
Ensinger draws the distinction that a batch record has to make. UL testing can be carried out to UL’s specifications or in a UL-accredited laboratory, while listing and Yellow Cards are handled by UL itself. A material with a UL listing is therefore not the same as a material that only complies with the requirements of a UL classification without a listing. If a listed material is required, Ensinger asks buyers to consult its sales team before ordering, because specific raw materials may have to be used.
Ensinger’s own data sheets show the difference in print. Its European sheet for TECAPEEK natural reads V-0 with the note “listed (value at 1.5mm)”. The carbon-filled grade’s sheet reads V-0 “corresponding to” DIN IEC 60695-11-10, without a listing note. On the US sheet, TECAPEEK natural shows V-0 without a thickness and adds a pass to FAR 25.853 at 3 mm (0.12 in), an aircraft test.
For the record, the wording matters more than the class. “Listed at 1.5 mm” can be checked against a card. “Corresponding to” is the maker’s statement, which may be correct but is a different kind of evidence.
Listed and compliant are different claims. A batch record should say which one it relies on, and quote the maker’s wording exactly.
Machining the Batch Without Losing the Rating
The flame-retardant additives that make the rating possible can change the shop rules. MCAM’s machining guide is direct about TIVAR BurnGuard: it is not suitable for machining with liquid coolants and should be kept away from high-moisture environments during both machining and storage. The active flame-retardant components may react with water- or oil-based coolants and create corrosive conditions that can damage steel machine components and tooling. Dry machining is recommended, with compressed air or an air spray as the only cooling.
That rule becomes a line in the batch record, because it is easy to break on a machine set up for wet cutting. The other machining points follow from the published properties.
- Wall thickness. A pocket, slot or chamfer that brings a wall below the thickness at which the grade holds V-0 takes that wall outside the printed rating. The thinnest finished wall belongs in the record beside the rated thickness.
- Heat. Röchling’s Flametech grade softens at a Vicat temperature of 79 °C (174 °F) and melts at 130 to 135 °C (266 to 275 °F), so frictional heat from a dull tool is a real risk to the surface.
- Size. At 150 to 230 × 10⁻⁶/K, a 500 mm (19.7 in) liner changes length by about 0.75 to 1.15 mm (0.030 to 0.045 in) for a 10 K difference between the shop and the inspection room.
- Storage. MCAM’s moisture warning applies to the stock and the finished parts alike, so parts wait for inspection and shipment in a dry place.
MCAM adds the general rule for UHMW-PE that also suits these grades: maximum feed and speed to move swarf, large tool clearances, and an air blast or vacuum to stop chip wrap.
The Batch Record, Line by Line
Ensinger describes the traceability it builds into its own stock. Material designations and product batch numbers stay recognizable on the semi-finished products in storage and handling, so each piece can be identified and traced. It issues certifications only on an order-specific basis and in connection with the material actually supplied, and it can provide test certificates to EN 10204, including a works test certificate of type 3.1 with tests from its own laboratories.
A machined batch extends that chain by one step. Table 3 lists what the record holds and who issues each item.
| Record item | Issued by | Where it comes from |
|---|---|---|
| Grade name and color | Stock maker | Data sheet and delivery note |
| Flame class and minimum thickness | UL, or the maker for a compliance statement | Yellow Card in Product iQ, or the maker’s sheet with its exact wording |
| Listing status | UL | Listed with a card, or complies without listing |
| Stock lot or batch number | Stock maker | Marking on the stock and the certificate |
| Material certificate | Stock maker | Type agreed at order, for example EN 10204 3.1 |
| Machining record | Machine shop | Dry machining for grades that require it; tools; date |
| Thinnest finished wall | Machine shop | Inspection report against the rated thickness |
| Storage and packing | Machine shop | Dry storage note where the maker requires it |
Each row answers a question an approval body or a customer’s quality team will ask. The two shop rows are the ones most often missing, because the stock certificate arrives complete and the machining adds nothing to it unless someone writes it down.
Planning the Batch and the Repeat Order
A flame-retardant batch is planned around its stock lot as much as around its machine time. The simplest record is one in which every part of the batch comes from one certified lot of one listed grade in one color, so that a single certificate and a single card reference cover the whole delivery. Where a batch has to draw on two lots, each part or each package carries its lot, and the record lists both.
The color column on the card turns into a purchasing rule. A grade recognized in one color is not automatically recognized in another, and the card’s own color code says which colors it covers. Any repeat order placed months later has to name the same grade, the same color and the same listing status, or the new batch is a new record rather than a copy of the old one.
Ensinger explains why the stock side of this matters. Its traceability works by upstream tracing, so that the cause of a problem with a component or a material can be found quickly and other affected customers can be told. That only works downstream if the machine shop keeps the lot identity through sawing, machining, inspection and packing, including on offcuts that may be used for a later batch.
The makers’ sheets also set the limit of what a data sheet promises. Röchling states on its Flametech sheet that the values are averages from regular statistical tests, in accordance with DIN EN 15860, provided for information and not binding unless expressly agreed in a contract of sale. A batch that needs a guaranteed property, rather than a typical one, needs that property named on the order and on the certificate.
- Name the grade, the color and the listing status on every repeat order.
- Ask for the certificate type at order, since makers issue certificates against the material actually supplied.
- Keep offcuts identified by lot if they may be used later.
- Record the dry-machining rule on the shop traveler for grades that require it.
Inspection and Release of a Flame-Retardant Batch
Inspection of a flame-retardant batch is ordinary dimensional inspection with three additions: the thinnest wall is measured and recorded, the parts are checked for coolant residue where the grade forbids liquids, and the lot number on the parts or their packaging is matched to the certificate. None of these adds a flame test. The rating comes from the material record.
A flame test on machined parts is a separate decision, usually driven by the end product. If one is needed, the calendar should allow for UL’s conditioning of two days at 23 °C (73 °F) and 50 % relative humidity before the vertical test, plus the time of the laboratory itself.
Some industries ask for different fire tests altogether. Ensinger names DIN 5510-2 for German railway components, replaced by the European standard EN 45545, and FAR 25.853 for aircraft, both of which add smoke density and toxicity under radiant heat and flame to pure combustibility. Röchling’s ASTM sheet cites an MSHA approval for underground mining. A UL 94 V-0 record does not answer any of these, and the purchase order should say which one the batch needs.
The flame class is settled before the first chip. What the shop adds to the record is proof that the right lot was cut, dry where required, and that no wall went thinner than the rating allows.
For flame-retardant parts made in batches for a product that is already approved, low-volume plastic CNC with bridge production keeps the same listed grade, the same lot records and the same dry machining rule from the first batch to the last.
Sources and Further Reading
- Combustion (Fire) Tests for Plastics, UL Solutions
- How to Read the UL Solutions Yellow Card, UL Solutions
- Color Codes and Abbreviations for Plastics Recognition, UL Solutions
- Plastics Recognition Program, Yellow Card eGuide, UL Solutions
- TIVAR BurnGuard UHMW-PE, Mitsubishi Chemical Advanced Materials
- Guide to machining plastic parts, metric system, 2026, Mitsubishi Chemical Advanced Materials
- Technical Data Sheet, Polystone M Flametech AST black, version 3.0, 2025, Röchling
- Technical Data Sheet, Polystone M flame retardant, ASTM, version 1.0, 2024, Röchling
- Frequently asked questions, machinable plastics, Ensinger
- PEEK unfilled, TECAPEEK natural (European data), Ensinger
- PEEK unfilled, TECAPEEK natural (US data), Ensinger