Conditioning

Conditioning is holding a plastic part or specimen at a set temperature and humidity until it is stable, before it is tested, measured or used.

Every Conditioning article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Conditioning is holding a plastic part or specimen at a set temperature and humidity until it is stable, before it is tested, measured or used. On a machined part it starts before the cut: nylon or acetal stock takes up water in the warehouse, and the machined part keeps settling in size after cutting as it reaches the humidity of its use. The same bar can give different sizes, hardness and electrical values depending on whether it is dry or conditioned. A drawing or a test report that states the conditioning removes that doubt.

Moisture State

Plastics Technology describes molded nylon as leaving the mold below about 0.2 % moisture, the dry-as-molded state, and then climbing toward 1.5 to 2 % in normal room air. Unfilled nylon 6 or 6/6 grows about 0.5 to 0.6 % as it does. Many molders condition their nylon parts deliberately, which shortens the time to equilibrium from weeks or months to a couple of days. Ensinger notes that moisture uptake and release cause swelling or shrinkage, and that conditioning may be recommended before processing.
Read More

Test Conditions

Stock data sheets print their conditioning beside the values. Ensinger prints the humidity beside electrical values on its PA6 sheet: resistivity at 23 °C and 12 % relative humidity, dielectric strength at 23 °C and 50 %. Where a sheet prints no condition, as some water absorption rows do, the value cannot be placed against another.

Storage

Ensinger stores semi-finished products flat, in closed rooms at 23 °C (73 °F) and 50 % relative humidity where possible, and asks that stock kept in the cold be given time to reach room temperature before machining. Storage is conditioning by another name: the bar arrives at the saw in whatever state the warehouse left it.

Drawing Callout

A machined nylon part can be inspected as machined, after a stated time at a stated temperature and humidity, or after drying. Plastics Technology makes the point for molded nylon that processor and customer have to agree the measuring conditions for first-article approval, and the same applies to machined parts. One line on the drawing settles it.

A Flame-Retardant Machined Plastic Batch and Its UL 94 V-0 Record

A machined batch carries a UL 94 V-0 rating only through its record of grade, color, thickness, listing and lot, plus proof the shop cut it dry and thick enough.

What a UL 94 V-0 Record Covers for a Machined Plastic BatchThe record covers the material, not the part. Ensinger, a stock-shape maker, states that combustibility testing to UL 94 is generally performed on the raw material.

Flatness and Warp of Thin Machined Plastic Plates

Thin plastic plates bow when stress, heat, clamping or moisture act on one face more than the other, so flatness is planned through stock, sequence, rest and measurement.

Why Thin Machined Plastic Plates Lose FlatnessA thin plate loses flatness when the stresses on its two faces stop balancing. Mitsubishi Chemical Advanced Materials (MCAM) explains the mechanism in its machining guide: extrusion, molding and machining leave residual stresses inside a thermoplastic, and when material is removed or the part meets elevated temperatures, those stresses redistribute and cause warping or dimensional change.

Shore D and Rockwell Hardness on Plastic Stock Data Sheets

Shore D and Rockwell values on plastic stock sheets rank surface hardness under named methods, cannot be converted into each other, and bind a supplier only when agreed.

What Shore D and Rockwell Numbers Mean on a Plastic Stock Data SheetBoth numbers rank how strongly a plastic resists a hard indenter pressed into its surface at room temperature. Neither is a strength, a wear rating or a design value.

Inspecting a Batch of Machined Plastic Parts Before It Ships

Inspecting machined plastic means stating the temperature, the probe force and the sample size, because a plastic part changes with all three.

How to Inspect a Batch of Machined Plastic PartsInspect the batch at a stated temperature, with a low-force or non-contact method for soft or thin parts, on a sample whose size is chosen in advance, and record the conditions with the results. Those four elements separate a measurement that can be repeated from one that cannot.

ASTM D638 Tensile Strength on Plastic Stock Data Sheets

A tensile figure on a data sheet belongs to one bar, one speed and one reading, so the sheet has to name all three before the number guides a design.

What ASTM D638 CoversThe scope of ASTM D638, Standard Test Method for Tensile Properties of Plastics, is the determination of the tensile properties of unreinforced and reinforced plastics in the form of standard dumbbell-shaped specimens, tested under defined conditions of pretreatment, temperature, humidity and testing machine speed. On astm.org the 2022 edition is listed as active.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.

Request a Quote