Isopropyl Alcohol

Isopropyl alcohol is the cleaning fluid that Mitsubishi and Quadrant name for washing amorphous plastic parts right after they have met a coolant.

Every Isopropyl Alcohol article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Isopropyl alcohol is the cleaning fluid that Mitsubishi and Quadrant name for washing amorphous plastic parts right after they have met a coolant. The wash is followed by a rinse in pure water. It protects polycarbonate, PSU, PPSU and PEI against stress cracking started by cutting fluid left on the surface. It cleans the surface and leaves the stress in place.

Wash Sequence

The guides place the wash immediately after machining with coolant. Mitsubishi’s wording for amorphous grades is to clean the part with isopropyl alcohol and then rinse it with pure water. The cases where a coolant cannot be avoided are named: deep holes and tapping. Everywhere else the same guides prefer pure water or compressed air as the coolant, so no wash is needed.
Read More

Limit

The annealing guides treat the wash as a separate protection against the same cracking. It removes the fluid but leaves the stress in the part. Where a part is heavily machined or will meet solvents in service, the stress is relieved by an anneal as well. The more material an amorphous part loses to the cutter, the stronger the case for annealing it.

Release Check

The wash belongs to the release of a batch. An inspection plan for amorphous parts machined with coolant lists the wash and rinse as done before packing. Without that line, a part can leave the room clean to the eye and crack later at the customer. A drawing for a PEI part can also state which cleaning fluids the part will accept in service. That line carries the same protection past delivery.

Drilling Deep Holes in Plastic Without Melting or Cracking

Holes deeper than two diameters trap heat in plastic, so drill grind, peck cycle, coolant choice and cool-down decide whether the part cracks or holds its size.

How to Drill a Deep Hole in Plastic Without Melting or CrackingTreat any hole deeper than two diameters as a cooling problem first and a cutting problem second. Both Mitsubishi Chemical Advanced Materials (MCAM) and Ensinger name the same threshold: heat builds very easily once the depth passes twice the diameter.

Inspecting a Batch of Machined Plastic Parts Before It Ships

Inspecting machined plastic means stating the temperature, the probe force and the sample size, because a plastic part changes with all three.

How to Inspect a Batch of Machined Plastic PartsInspect the batch at a stated temperature, with a low-force or non-contact method for soft or thin parts, on a sample whose size is chosen in advance, and record the conditions with the results. Those four elements separate a measurement that can be repeated from one that cannot.

Annealing Machined Plastic Parts Between Roughing and Finishing

Annealing between roughing and finishing trades oven days for flat, stable parts, and it pays only when stress, shape or tolerance demand it.

When a Machined Plastic Part Needs AnnealingA machined plastic part needs an intermediate anneal when it has tight tolerances, an asymmetric shape, or a large share of its blank removed, and when it does not need one the stock maker has already done the work. Ensinger states the starting condition: its semi-finished products are always annealed after production, which is why a first cut can start without a stress-relief step.

PEI Ultem Stock for CNC Machined Parts

PEI holds stiffness and shape at heat, and it asks for dry cutting, careful fluids and an annealing decision before the first part is cut.

PEI Ultem Properties for Machined PartsPolyetherimide, PEI for short, is an amorphous thermoplastic, and Ensinger, which extrudes it into rod and plate, notes that it is commonly referred to as ULTEM plastic after the resin's trade name. Ensinger describes the material as having high mechanical strength and rigidity, exceptional creep resistance over a wide temperature range and very good hydrolysis resistance, and as inherently flame retardant with low smoke emission, which makes it a preferred material for aircraft interiors.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.