Meaning

Flatness is how closely a machined face follows a true plane. On plastic plate it is most often lost when one side alone is cut. It is held by stock choice, balanced cuts, rest or anneal, and a light final pass. It is lost by one-sided removal, hard clamping and uneven heat.

Bow Mechanism

Mitsubishi shows a plate machined on one side bowing top and bottom about the centerline of the extrusion. The stress released on the cut side is no longer balanced by the other. Röhm notes the same for acrylic: treating only one surface mechanically can distort the sheet slightly. Its remedy is an anneal, which reverses the distortion.
Read More

Anneal Sequence

Mitsubishi’s guide gives the path for a tight flat on an uneven contour: rough, anneal or rest, and finish with a light cut, removing material equally on both sides of the centerline. Improved flatness comes from rough machining, annealing and finish machining with a very light cut. Mitsubishi describes the same sequence. Parts are fixtured to the desired flatness through the whole cycle and stay fixtured until cool to the touch.

Second Clamp

A part that bowed cannot be pulled flat for the second side without a cost. The holding article in these resources gives an illustration with a bow of a fifth of a millimeter (0.008 in). A vacuum plate or vise pulls the part flat, the cutter cuts it flat, and it springs back by about the same amount when released. Measuring the rested part before it is clamped shows whether it bowed. The finishing pass is then taken at light depth.

First-Part Check

On a part with one-sided pockets, the plan measures flatness across the open side on the first part. It measures again after the rest. A drawing that asks for flatness on such a plate is asking for stress relief or balanced cuts around the centerline.

Flatness and Warp of Thin Machined Plastic Plates

Thin plastic plates bow when stress, heat, clamping or moisture act on one face more than the other, so flatness is planned through stock, sequence, rest and measurement.

Why Thin Machined Plastic Plates Lose FlatnessA thin plate loses flatness when the stresses on its two faces stop balancing. Mitsubishi Chemical Advanced Materials (MCAM) explains the mechanism in its machining guide: extrusion, molding and machining leave residual stresses inside a thermoplastic, and when material is removed or the part meets elevated temperatures, those stresses redistribute and cause warping or dimensional change.

Machining PEEK Unfilled and Carbon-Filled Stock

Unfilled and carbon-filled PEEK share a polymer but differ in stiffness, conductivity, tooling, cutting data and tolerance, so the grade belongs on the drawing.

How Unfilled and Carbon-Filled PEEK Stock Differ for Machined PartsUnfilled PEEK machines like a hard, stiff thermoplastic: short chips, little burr, high feed rates and fine finishes. Carbon-filled PEEK machines like a composite: abrasive to tools, sensitive to fiber direction, and best cut with carbide or diamond at lower speeds.

Inspecting a Batch of Machined Plastic Parts Before It Ships

Inspecting machined plastic means stating the temperature, the probe force and the sample size, because a plastic part changes with all three.

How to Inspect a Batch of Machined Plastic PartsInspect the batch at a stated temperature, with a low-force or non-contact method for soft or thin parts, on a sample whose size is chosen in advance, and record the conditions with the results. Those four elements separate a measurement that can be repeated from one that cannot.

Holding Plastic Parts for CNC Machining Without Bending Them

Plastic parts distort under clamps that metal parts shrug off, so the hold, the support and the symmetry of the cut set the final size.

How to Hold a Plastic Part on a CNC MachineHold it on as much surface as the geometry allows, with the lowest force that keeps it from moving, and with every thin wall backed by something solid. That sentence compresses three recommendations that recur across the stock-shape makers' guides: light clamping, support under the cut, and distribution of the force by vacuum or soft jaws instead of point contact.

Annealing Machined Plastic Parts Between Roughing and Finishing

Annealing between roughing and finishing trades oven days for flat, stable parts, and it pays only when stress, shape or tolerance demand it.

When a Machined Plastic Part Needs AnnealingA machined plastic part needs an intermediate anneal when it has tight tolerances, an asymmetric shape, or a large share of its blank removed, and when it does not need one the stock maker has already done the work. Ensinger states the starting condition: its semi-finished products are always annealed after production, which is why a first cut can start without a stress-relief step.

Machining Tolerances by Part Size for Engineering Plastics

Published plastic tolerances widen with feature size and split by polymer group, so a drawing has to state size, grade, temperature and rest.

Published Machining Tolerances by Feature Size and Material GroupTable 1 reproduces the Mitsubishi table for nine of its sizes, with inches beside each figure. The five groups are the guide's own: HDPE; the group that holds PET-P, PC, PEEK, PTFE 500, PPS, PEI, PPSU and PSU; the group that holds PA, POM and PTFE 207; PEEK with fillers; and PAI with PBI.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.

Request a Quote