Water Absorption

Water absorption is the share of its weight a plastic takes up in water, measured under ASTM D570 after 24 hours and at saturation.

Every Water Absorption article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Water absorption is the share of its weight a plastic takes up in water, measured under ASTM D570 after 24 hours and at saturation. It is printed as a percentage of mass, not of length. It indicates how far humidity will move a part’s size over days and weeks.

Published Values

TECAFORM AH acetal copolymer lists 0.22 percent after 24 hours and 0.80 percent at saturation. Delrin 150 homopolymer lists 0.25 and 0.9 percent. Unfilled PEI lists 0.25 percent after 24 hours and 1.25 percent at equilibrium, five times the short figure. Glass dilutes the uptake, to 0.16 and 0.90 percent at 30 percent loading. The TIVAR 1000 UHMW-PE sheet gives nil, and the HDPE sheet slight.
Read More

Size Effect

None of the sheets gives a dimensional change per percent absorbed. The acetal article therefore asks that a part held to a close size be measured at the humidity it will live in. A PEI part measured fresh from the machine and again after weeks in humid air is not guaranteed to match. The thermal expansion article adds that moisture alters size over days to weeks, at a rate the sheets print as mass.

Range Across Grades

Polyethylene takes up almost no water, so heat is the movement to plan for there. Nylon sits at the other end of these resources. Quadrant names moisture swelling as mainly a nylon effect, along with PBI and PAI. Those grades are dried in a vacuum oven and stored in sealed bags with desiccant. Acetal takes up little water, which is part of why it holds size well.

Machining PEEK Unfilled and Carbon-Filled Stock

Unfilled and carbon-filled PEEK share a polymer but differ in stiffness, conductivity, tooling, cutting data and tolerance, so the grade belongs on the drawing.

How Unfilled and Carbon-Filled PEEK Stock Differ for Machined PartsUnfilled PEEK machines like a hard, stiff thermoplastic: short chips, little burr, high feed rates and fine finishes. Carbon-filled PEEK machines like a composite: abrasive to tools, sensitive to fiber direction, and best cut with carbide or diamond at lower speeds.

Cast and Extruded Nylon PA6 Stock for Machined Parts

Cast and extruded PA6 share a name but not their stress, crystallinity, chips or moisture behavior, and a machined nylon part keeps changing size after the cut.

Cast or Extruded PA6 for a Machined PartCast PA6 is usually the better machining stock when the part is large, flat, stiff or close-toleranced. Extruded PA6 is the tougher, more elastic choice for smaller parts where impact strength and elongation matter more than the last hundredth of a millimeter.

UHMW-PE and HDPE Stock for CNC Milling and Turning

UHMW-PE wears longest and HDPE holds shape better, and both need sharp tools, chip control and a stated measurement temperature to hold size.

UHMW-PE and HDPE Differences for Machined PartsBoth are polyethylene, and the difference starts with chain length. Mitsubishi describes its TIVAR 1000 Virgin UHMW-PE as setting the standard for ultra high molecular weight polyethylene shapes, with a combination of wear and corrosion resistance, a low-friction surface and excellent impact strength.

PEI Ultem Stock for CNC Machined Parts

PEI holds stiffness and shape at heat, and it asks for dry cutting, careful fluids and an annealing decision before the first part is cut.

PEI Ultem Properties for Machined PartsPolyetherimide, PEI for short, is an amorphous thermoplastic, and Ensinger, which extrudes it into rod and plate, notes that it is commonly referred to as ULTEM plastic after the resin's trade name. Ensinger describes the material as having high mechanical strength and rigidity, exceptional creep resistance over a wide temperature range and very good hydrolysis resistance, and as inherently flame retardant with low smoke emission, which makes it a preferred material for aircraft interiors.

Acetal Homopolymer and Copolymer Stock for CNC Machined Parts

Homopolymer is stiffer and harder, copolymer is sold porosity-free with less water uptake and less thermal growth, and the stock a part is cut from decides which it inherits.

Acetal Homopolymer and Copolymer Differences in Machined PartsAcetal, the polyoxymethylene or POM family, reaches a machine shop as two chemistries. Homopolymer chains repeat one unit; copolymer chains carry two.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.

Request a Quote