Rest Time After Machining

Rest time after machining is the stated wait between the last cut and inspection.

Every Rest Time After Machining article of the Plastic CNC Resources, newest first, each written from published standards, research and makers’ data.

Meaning

Rest time after machining is the stated wait between the last cut and inspection. It keeps cutting heat and early stress release out of the reading. The thermal expansion and drilled hole articles in these resources both ask for it on the drawing. Without it, two measurements of one part can differ by more than its tolerance.

Reason

A fresh plastic part is still changing. Heat from the cut leaves it warm, so the first measurement reads large. Stress released by the removal of material shifts it over hours. Moisture alters its size over days to weeks, at a rate the sheets print as mass, not length. Mitsubishi’s turning tips add that most diameters grow after cutting.
Read More

Overlapping Effect

All three effects can overlap on one freshly cut part. A first-article measurement taken at the machine, warm and fresh, is not the size the part keeps. One taken after rest, at the stated temperature, is. A hole is the clearest case. It moves with heat and with stress, so the hole call-out carries both a measurement temperature and a rest time.

Drawing Note

The thermal expansion article gives a model line. Dimensions apply at 20 °C (68 °F) after 24 hours at that temperature. The line fixes the rest and the soak at once. It also gives a supplier and a buyer the same starting point for any later dispute.

Record Entry

The inspection article treats time since machining as the third condition of a plastic measurement, after temperature and probe force. The record states whether a part was measured as machined, after a rest, after drying or after conditioning. A reading without that line cannot be compared with the next one.

Flatness and Warp of Thin Machined Plastic Plates

Thin plastic plates bow when stress, heat, clamping or moisture act on one face more than the other, so flatness is planned through stock, sequence, rest and measurement.

Why Thin Machined Plastic Plates Lose FlatnessA thin plate loses flatness when the stresses on its two faces stop balancing. Mitsubishi Chemical Advanced Materials (MCAM) explains the mechanism in its machining guide: extrusion, molding and machining leave residual stresses inside a thermoplastic, and when material is removed or the part meets elevated temperatures, those stresses redistribute and cause warping or dimensional change.

Thermal Expansion of Machined Plastic Parts by Material and Size

Every machined plastic dimension has a temperature, and the material decides how many degrees of drift a given tolerance can absorb.

Thermal Expansion of Machined Plastic Parts per 10 DegreesThe coefficient of linear thermal expansion, CTE, is the fractional length change per degree. Plastic sheets print it in 10⁻⁶ per kelvin or in inches per inch per degree Fahrenheit, and the two convert by a factor of 1.8: one in/in/°F is 1.8 per °C.

Request a Plastic CNC Quote

Send the 2D drawing and the 3D file, with the quantity and the stage of the project. An engineer replies within 1 working day.

The quote form, the mutual NDA and the private folder for your files are on Protolis Atelier, with Plastic CNC chosen.