Meaning
The glass transition is the temperature range in which a plastic’s amorphous regions turn from hard and glassy to soft and rubbery. Data sheets print it as Tg. Above it, a plastic loses stiffness and can shrink or deform when it cools again. For machining, it marks how much frictional heat a part can take before its structure changes.Typical Values
Ensinger prints Tg to DIN EN ISO 11357 on its stock sheets: 150 °C (302 °F) for unfilled TECAPEEK natural, 147 °C (297 °F) for the carbon-filled grade and 151 °C (304 °F) for the ceramic-filled grade. Its extruded PA6, TECAMID 6 natural, lists 45 °C (113 °F). The value depends on the polymer and, for nylon, on how much water it holds.Read More
Effect of Water
Water acts as a plasticizer in nylon. Plastics Technology explains that it lowers the glass transition of nylon 6 and 6/6 from 65 to 70 °C (149 to 158 °F) in the dry state to about 10 °C (50 °F) when the material has absorbed moisture. That is why dry nylon feels brittle in a cold, dry winter and conditioned nylon feels tough, and why the moisture state belongs beside any mechanical value.Machining Heat
Ensinger warns that heat input above the glass transition causes microstructural change and post-shrinkage when the part cools. Its figures for the potential are about 1.0 to 2.5 % for semi-crystalline plastics and 0.3 to 0.7 % for amorphous ones, and it notes that shrinkage and warping show most in asymmetric parts. A hot pocket on one face of a thin plate is the classic case: the overheated face shrinks and the plate bows. Sharp tools, a properly loaded cut and good chip removal keep the cutting zone below the point where this happens.